2015 — Mapping iron gall ink penetration within paper fibres using scanning transmission X-ray microscopy. Journal of Analytical Atomic Spectrometry vol. 30, , p. 635-641
,
2015 — Alteration of fossil-bearing shale (Autun, France; Permian), part II: Monitoring artificial and natural ageing by combined use of S and Ca K-edge XANES analysis, Rock-Eval pyrolysis and FTIR analysis. Annales de Paléontologie vol. 101, n° 3, p. 225-239
,
2015 — Alterations of fossil-bearing shale (Autun, France; Permian), part III:Framboidal pyrite and sulfur as the main cause of efflorescence. Annales de Paléontologie , ,
,
2015 — « Counterfeit coinage of the Holy Roman Empire in the 16th century: silvering process and archaeometallurgical replications » in Archaeometallurgy in Europe III.. , ,
,
2015 — Alteration of fossil-bearing shale (Autun Basin, France; Permian), part I: Characterizing iron speciation and its vulnerability to weathering by combined use of Mössbauer spectroscopy, X-ray diffraction, porosimetry and permeability measurements. Annales de Paléontologie vol. 101, n° 2, p. 75-85
,
mars 2014 — The Dutch Fe-Migration Mending Test : Exploring Further Areas of Use. Journal of Paper Conservation vol. 15, n° 1, p. 9-15
,
2014 — Paper strengthening by polyaminoalkylalkoxysilane copolymer networks applied by spray or immersion: a model study. Cellulose vol. 21, , p. 705-715
,
2014 — Accelerated ageing of shales of palaeontological interest: Impact of temperature conditions. Annales de Paléontologie vol. 100, , p. 137-149
,
2014 — Un nouvel outil pour évaluer le risque de migration d’encres ferrogalliques : possibilités et limites. Support Tracé vol. 14, ,
,
2014 — The Impact of Gelatine Sizing on Globe Varnishing. Journal of Paper Conservation vol. 15, n° 3, p. 7-13
,
août 2013 — Étude de collections de paléontologieDe la caractérisation à la reproduction desaltérations de fossiles dits pyriteux. Conservation, Exposition, Restauration d’Objets d’Art , ,
,
juin 2013 — Damaged Blue Papers : Optimising Consolidation while Preserving Original Colour. Journal of Paper Conservation vol. 14, n° 2,
,
2013 — The use of halide charged interleaves for treatment of iron gall ink damaged papers. Polymer Degradation and Stability vol. 98, , p. 1339-1347
,
2013 — Étude pluridisciplinaire du squelette de rhinocéros laineux, Coelodonta antiquitatis (Blumenbach, 1799), de l’Institut de paléontologie humaine (Paris, France). L’anthropologie vol. 117, , p. 1-47
,
2013 — Identification of synthetic dyes in early colour photographs using capillary electrophoresis and electrospray ionisation-mass spectrometry. Talanta vol. 114, , p. 217-226
,
septembre 2012 — Methods of Aqueous Treatments : The Last Resort for Badly Damaged Iron Gall Ink Manuscripts. Journal of Paper Conservation vol. 13, n° 3, p. 7-13
,
février 2012 — Reinforcement properties of 3-aminopropylmethyldiethoxysilane and N-(2-Aminoethyl)-3-aminopropylmethyldimethoxysilane on polyurethane ester foam. Polymer Degradation and Stability vol. 97, n° 11, p. 2340-2346
,
2012 — Raman and FTIR spectroscopy applied to the conservation report of paleontological collections: identification of Raman and FTIR signatures of several iron sulfate species such as ferrinatrite and sideronatrite. Journal of Raman Spectroscopy vol. 43, , p. 1265-1274
,
2012 — An Aqueous Treatment for Highly Damaged Manuscripts: Minimising the Risk of Mechanical damage. Journal of Paper Conservation vol. 13, n° 3, p. 36-37
,
septembre 2011 — Combining XANES, ICP-AES, and SEM/EDS for the study of phytate chelating treatments used on iron gall ink damaged manuscripts. Journal of Analytical Atomic Spectrometry , ,
,